MEMSnet Home: MEMS-Talk: Breakdown voltage of thermal oxide
Breakdown voltage of thermal oxide
2003-07-23
Rahul Saini
2003-07-24
Gormley, Colin
2003-07-24
Jobert van Eisden
Breakdown voltage of thermal oxide
Gormley, Colin
2003-07-24
It is generally considered to me 10MV/cm for thermal oxide.

-----Original Message-----
From: Rahul Saini [mailto:[email protected]]
Sent: 24 July 2003 00:17
To: [email protected]
Subject: [mems-talk] Breakdown voltage of thermal oxide


Hi,

I want to know the breakdown voltage of 2um thick thermal BOX for a SOI
wafer. I am looking for some reference or an equation to determine the
breakdown voltage with thickness for thermal oxide. Has anyone done any
characterization for calculating the breakdown voltage?


Thanks,
Rahul

MEMS Engineer
Zyvex Corporation
972-235-7881 Ext 266




_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing