Hi, dear colleagues,

Does anybody know the annealing condition for SiN on a sacrifical SiO2
layer? Basically we found a very strong residual stress in the SiN layer
of our wafers and want to reduce it as much as possible by annealing.

Thanks and appreciate your reply!

Changping