Hallo,
does anyone know if there is a photoresist or
photosensitive polymmide that can resist a 30 hour
etch in KOH or TMAH?
Can you also suggest the best etching conditions for
the highest selectivity for that matirial and silicon?
Thank you very much.

Michele

______________________________________________________________________
Yahoo! Mail: 6MB di spazio gratuito, 30MB per i tuoi allegati, l'antivirus, il
filtro Anti-spam
http://it.yahoo.com/mail_it/foot/?http://it.mail.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
University Wafer