MEMSnet Home: MEMS-Talk: Gold plating
Gold plating
2003-07-26
sriramb
2003-07-28
Rick Morrison
2003-07-28
[email protected]
2003-07-28
Michael D Martin
Gold plating
Michael D Martin
2003-07-28
You need an adhesion layer. Use ~250 angstroms of Cr, Ti, or Ta.

-Mike


>>> [email protected] 07/26/03 02:42AM >>>
Dear All,

I tried to plate Gold over a Platinum thin film (3000 Angstrom) on
SiO2.
Before the plating, we go through a degreasing step, wherein we boil
the
Silicon wafers in Tri Chloro Ethylene, followed by a dilute HCl dip.
The Pt film is deposited by DC sputtering.

The trouble is that the Pt film peels off when the HCl dip is done.

What should I do to overcome this problem?

Thanks in advance.

Thanking You,
With Best Regards,
Sriram
Senior Process Engineer,
BEL Bangalore
INDIA



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.