MEMSnet Home: MEMS-Talk: Etch rate of Cu in BHF
Etch rate of Cu in BHF
2003-07-29
Frank Rasmussen
2003-07-29
Kirt & Erika Zipf-Williams
Etch rate of Cu in BHF
Kirt & Erika Zipf-Williams
2003-07-29
For evaporated copper in 5:1 BHF, we measured an etch rate of less than 5
nm/min,
with the the surface being slightly roughened.
    --Kirt Williams, Ph.D.    consultant

----- Original Message -----
From: Frank Rasmussen 
To: 
Sent: Tuesday, July 29, 2003 8:05 AM
Subject: [mems-talk] Etch rate of Cu in BHF


> Hi,
>
> Does anyone know the (approximate) etch rate of Cu in BHF ?
>
> I am using BHF to remove a copper oxide layer generated on my structures
during processing. I expect the Cu etch rate to be very small, though I
would like to have this confirmed.
>
> The Cu on my wafers have been deposited by means of MOCVD. Perhaps this is
relevant to the question above ?
>
> Thanks,
> Frank
>
> __________________
> Frank Engel Rasmussen
> Industrial PhD Student
> MicroElectro-Mechanical Systems (MEMS) Group
>
> Mikroelektronik Centret
> Technical University of Denmark
> Oersteds Plads, Bldg. 345-east
> DK-2800 Kgs. Lyngby, Denmark
>
> Tel. direct: +45 4525 6316
> Tel. switchboard : +45 4525 5700
> Cell phone: +45 2682 3493
> Fax : +45 4588 7762
> E-Mail : [email protected]
> http://www.mic.dtu.dk
>
>
>


----------------------------------------------------------------------------
----


> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Mentor Graphics Corporation