A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Piezoresistor alignment
Piezoresistor alignment
2003-07-30
sriramb
Piezoresistor alignment
sriramb
2003-07-30
Hello All,

         I am trying to fabricate Piezoresistive Pressure Sensors, as
part of the project work associated with my part-time Master's Degree. I
need to know how exactly to orient the P type piezoresistors in the [110]
direction. I work on 100mm diameter, {100} orientation, N type Silicon
wafers. The resistors are formed by Boron Ion Implant into the silicon
substrate.

         Presently, I align the primary wafer flat parallel to the mask
edge (the piezoresistors are parallel to the mask edge). This is however
only an approximate method of alignment, and the resistors do not align
exactly in the [110] direction. This inturn affects the output of my
resistive Wheatstone bridge.

Could someone suggest a method that can repeatedly be used to exactly
align the resistors (on a 100mm silicon wafer) in the [110] direction?
It would be a great help.

Thanks in advance.

With Best Regards,
Sriram
Senior Process Engineer,
Bharat Electronics
Bangalore 560 013
INDIA



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMS Technology Review