Silicic acid for TMAH etch
2003-08-03
kris
2003-08-01
[email protected]
Mask Clean
Lin, Yaojian
2003-07-31
Hello Friends,

I am looking for the methods to clean the dirty mask, which may have some
polymer spots.

Could you please give me some clue?

With many thanks,

Yaojian Lin




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.
University Wafer