Ag adhesion
2003-08-05
Mark Leonard
2003-08-05
Hongjun Zeng
2003-08-05
Kirt & Erika Zipf-Williams
2003-08-05
Michael D Martin
Ag adhesion
Michael D Martin
2003-08-05
I've had successfull sputtered Ag adhesion using ~250nm Cr on a
polyimide substrate. My silver layers were only 0.1 microns though. Such
a thick film may have some serious stress issues.

-Mike


>>> [email protected] 08/05/03 06:23AM >>>
Hi

We are having a few problems with a e-beam evaporated film of Ag, ~5-10
microns thick. We have tried putting a seed layer of Ti down onto glass
and Si but the Ag film just comes away from the Ti. Can anyone suggest a
better seedlayer onto glass or Si before we deposit the Ag

Many thanks

Mark Leonard
Electrical, Electronic and Computer Eng,
Mountbatten Building,
Heriot Watt University
Riccarton
Edinburgh EH14 4AS
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
University Wafer
Process Variations in Microsystems Manufacturing
MEMStaff Inc.