Density measurement
2003-08-06
anshu mehta
2003-08-06
John Fijol
2003-08-06
David Nemeth
Density measurement
David Nemeth
2003-08-06
If you have a crystal monitor in your deposition system, you could compare
the crystal monitor reading to a thickness measurement done on a step edge
using a profilometer.  You'd have to have a reasonable guess at the acoustic
impedance - I don't know how much uncertainty that would introduce if there
was an error in that parameter.

David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA


-----Original Message-----
From: mems-talk-bounces+nemeth=sophiawireless.com@memsnet.org
[mailto:mems-talk-bounces+nemeth=sophiawireless.com@memsnet.org]On
Behalf Of anshu mehta
Sent: Wednesday, August 06, 2003 4:08 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Density measurement


Hi!

Does anyone have suggestions on ways to measure
density for thin films?

Thanks,
Anshu.


________________________________________________________________________
Send free SMS using the Yahoo! Messenger. Go to
http://in.mobile.yahoo.com/new/pc/

_______________________________________________
MEMS-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Nano-Master, Inc.
Tanner EDA by Mentor Graphics