Ag-AgCl electrode
Stefan Fiedler
2003-08-06
Hi,
Please look at "Fabrication and characterization of a new planar solid-state
reference electrode for ISFET sensors
by Huang, I.-Y. / Huang, R.-S., in Thin Solid Films, 406 ( 2002) 255-261.
See also: "Improvement of integrated Ag/AgCl thin-film electrodes by KCl-gel
coating for ISFET applications" by
Huang, I.-Y. / Huang, R.-S. / Lo, L.-H., in Sensors and Actuators B 94 (2003)
53-64
Herein some literature overview on the topic, including earlier work by
M. Steyaert, M. Lambrechts and W. Sansen on "Noise power spectrum density
analysis of planar Ag/AgCl electrodes"
in Sensors and Actuators 12 1987 185-192
and L. J. Bousse, P. Bergveld and H. J. M. Geeraedts on "Properties of Ag/AgCl
electrodes fabricated with IC-compatible technologies"
Ibid, 9 1986 179-197

Would be interested in results of your further search for strategies / summary
of the mems-group-discussion.
Might be you could pass it along?

Best regards
. . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . .
 Dr. Stefan Fiedler
 Fraunhofer - Institut fuer
 Zuverlaessigkeit u. Mikrointegration
 Gustav-Meyer-Allee 25
 D-13355 Berlin
 Germany

 Telefon +49 (0) 30/46403-217
 Telefax +49 (0) 30/46403-271
 e-mail  [email protected]
 http://www.izm.fhg.de
. . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . . .



Hiroaki SUZUKI wrote :

> Hi all
>
> Has anyone tried to pattern an Ag-AgCl electrode on either glass or siliocon
> substrate? I deposited and patterned Ag and immersed in chlorine based bleach
> solution, but Ag easily peels off.
>
> Although Ag-AgCl electrode is very often used for the electrical detection of
> biological stuff, I don't see it in Bio-MEMS literatures. Most people use
> Ti/Au or Cr/Au electrode. But in my observation, Cr as an adhesion layer
> elutes when the current flows and the electrode peels off as well.
>
> Any suggestion/discussion would help.
> Thanks,
>
> ----------------------------
> Hiroaki SUZUKI
> The University of Tokyo
> Institute of Industrial Science (IIS)
> ----------------------------
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


fiedler.vcf (text/x-vcard, 375 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering