MEMSnet Home: MEMS-Talk: Glass-Glass thermal fusion bonding
Glass-Glass thermal fusion bonding
2003-08-11
Balaji Srinivasan Venkatesh
2003-08-12
Brubaker Chad
2003-08-28
Sooje Cho
Glass-Glass thermal fusion bonding
Brubaker Chad
2003-08-12
Balaji,
Glass to Glass does in fact bond via direct bond methods.  The temperature
required for final anneal is generally in the 275C to 350C range depending upon
the materials.  However, as in standard fusion bonding, the biggest issue is
roughness (local surface roughness) and flatness.  If the surface is too rough,
intimate contact cannot be created, and if the substrate is not flat enough,
intimate contact cannot be created across the entire surface.
In addition, glass is very hydroscopic, so unless care is taken during surface
activation, voids can occur after annealing, even if the pre-anneal condition is
void free.Here are the issues:
These comments apply to quartz, pyrex, Corning glasses, sapphire, and ordinary
soda lime glass.

If you have any further questions, feel free to contact me, or check out our web
site at www.evgroup.com.


Best Regards,
Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   Balaji Srinivasan Venkatesh [mailto:[email protected]]
Sent:   Monday, August 11, 2003 2:12 PM
To:     [email protected]
Subject:        [mems-talk] Glass-Glass thermal fusion bonding

Hi..
     I would like to do a Glass-Glass Fusion bonding  without any intermediate
layer ..Does it require any particular type of glass and can anybody let me know
the protocol for this kind of bonding.

Also any suggestion on UV Bonding of glass would be of help..

Thank You,
Balaji



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Addison Engineering
MEMS Technology Review