Carbon Nanotube Ultrasonication
2003-08-14
Husein Rokadia
2003-08-15
Soojin Oh
Carbon Nanotube Ultrasonication
Soojin Oh
2003-08-15
If your CNT is untreated (as synthesized), try a
non-polar solvent. Probably THF or Toluene will work
well. Or NMP is a good solvent if you don't need a
high vapor pressure of the solvent. 1mg/100mL is not a
very high concentration for a CNT suspension, but you
can make it even more dilute.

Soojin
Chapel Hill

--- Husein Rokadia  wrote:
> Hey Guys,
> I am trying to sonicate Multiwall Carbon Nantoubes
> in Isopropyl Alcohol.
> My current mixing ratio is 1mg of CNT /100 ml of IPA
> for about 2 hours.
> The problem with my current method is that the CNTs
> coagulate very quickly
> after I stop the sonication, I have tried to
> sonicate for a longer duration
> but to no avail.
>
> I am wondering if there is a problem with my
> concentration ratio, or if I
> should  switch to some other solvent?
> Alternately please suggest sonication recipies of
> your own.
>
> Thanking you in anticpation,
>
> Sincerely,
> Husein Rokadia
>
> Husein Rokadia
> University of Arkansas,
> MEEG Rm 223,
> O:479-575-6821
> R:479-871-0033
> Lab:479-575-4150
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
http://sitebuilder.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review