A.K.Ismail
2003-08-19
Dear all,

Does anybody know if a low temperature CVD oxide (i.e LPCVD or PECVD) can be
deposited on Pyrex substrate?. I would like to know if this CVD oxide can have
a good adhesion to pyrex. I found in literature almost people deposited CVD
oxide on Si substrate. I am expecting that it can have a good adhesion since
pyrex is also an oxide. Could anyone who has experience about this process can
confirm to me.

Thank you.

A.K.Ismail.



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing