A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Electrodes in Microchannel
Electrodes in Microchannel
2003-08-03
mems work
2003-08-11
Andreas Scheipers
2003-08-11
Brubaker Chad
2003-08-13
Tom Fan
2003-08-13
Ji'e (Jayne) Wu
2003-08-18
Andreas Scheipers
2003-08-18
Jochen Zöllin
2003-08-25
Andreas Scheipers
2003-08-13
Brubaker Chad
2003-08-26
Randy Grow
2003-08-26
Michael D Martin
2003-08-26
Brubaker Chad
Electrodes in Microchannel
Randy Grow
2003-08-26
Does anyone have a recommendation for a conformal layer of PMMA? I have
8 micron steps that have been difficult to cover. I have succeeded with
a  bilayer of PMMA, each layer being 1.6 microns, for a total of 3.2
microns. At that thickness, though, ebeam lithography becomes very
difficult.

Thanks,

Randy Grow
Ph.D. Candidate
Dept. of Applied Physics
Stanford University


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group