MEMSnet Home: MEMS-Talk: minority carrier lifetime measurement
minority carrier lifetime measurement
2003-09-11
Lau, Phil
2003-09-11
Jean-jacques Simon
minority carrier lifetime measurement
Lau, Phil
2003-09-11
Henry,

Try the following company:-


Charles Evans & Associates
810 Kifer Road
Sunnyvale, CA 94086
Voice: (408) 530-3500


Their email address is: [email protected]





-----Original Message-----
From: Helin Ji [mailto:[email protected]]
Sent: 10 September 2003 18:52
To: General MEMS discussion
Subject: [mems-talk] minority carrier lifetime measurement


*** WARNING ***

This mail has originated outside your organization,
either from an external partner or the Global Internet.
     Keep this in mind if you answer this message.

Does anyone know any company or university providing
minority carrier lifetime measurement service ?

Thanks

Henry


__________________________________
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
http://sitebuilder.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Mentor Graphics Corporation
Nano-Master, Inc.