2003-09-11
Veeco Metrology Group, Santa Barbara, CA, USA manufactures Scanning Spreading
Resistance Microscopy (SSRM) tools. You may contact them directly for your
specific requirements.

"thierry.bouchet"  wrote:Does anyone know
any company or university providing
SRP (Spreading Resistance Profile) ?

Thanks

Thierry Bouchet
R&D engineer
IBS
Rue gaston Imbert prolongée
tel: 04 42 53 89 64
fax: 04 42 53 89 59
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


(Pramod Gupta)

20800 Valley Green Dr., # 445

Cupertino, CA 95014

Phone: (408) 253-1646

---------------------------------
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Addison Engineering