Hi!
I have used  evaporated Chrome-Gold as the seed layer to electroplate Au and
suceeded. I would like to know if  it essential to have the Au layer on the
Chrome layer before I electroplate more Au?

Thanx,
Regards,
Husein Rokadia

_________________________________________________________________
A chance to meet Aishwarya Rai. http://www.myenjoyzone.com/msn/knk.php3 Win
lucky prizes.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering