MEMSnet Home: MEMS-Talk: BCB adhesive wafer bonding
BCB adhesive wafer bonding
2003-09-14
Richard Jiang
2003-09-16
Absara Micro Systems
BCB adhesive wafer bonding
Absara Micro Systems
2003-09-16
Hi Richard,

Use BCB part No. 4024 for adhesive bonding. I use this material for sensor
wafer bonding applications.
Gautham V
for ABSARA MICRO SYSTEMS (S) PTE LTD
17, Philips Street, # 05 - 01
Grand Building, Singapore - 048695

Ph: 65 68580585
Fax: 65 62822870

e-mail: [email protected]
website: www.absaramicro.com
----- Original Message -----
From: "Richard Jiang" 
To: 
Sent: Sunday, September 14, 2003 11:02 PM
Subject: [mems-talk] BCB adhesive wafer bonding


> Hi all,
>
> I am interested in MEMS wafer bonding using dry etch BCB or photo-BCB from
DOW
> Chemicals. Does anyone can tell me which BCB, dry etch BCB or photo-BCB,
is more
> easier to perform adhesive wafer bonding successfully?
>
> I want to bond a MEMS device and a silicon cap (with cavities etched in
it)
> together.
>
> Best regards,
>
> Richard Jiang
>
>
> =====
> Richard Jiang
>
> Shanghai Institute of Microsystem and Information Technology, CAS
> 865 Changning Road
> Shanghai 200050, China
> [email protected]
> Tel: 86-21-62511070-5966
>
> __________________________________
> Do you Yahoo!?
> Yahoo! SiteBuilder - Free, easy-to-use web site design software
> http://sitebuilder.yahoo.com
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.