Hi,

May i know if u have any metallisation on ur chips??

Kris
--- Áº µÏ  wrote:
> Dear MEMSers,
> I need to use TMAH etch Si for just 2-3 microns, but
> want to be as smooth
> as possible.
> Dose anyone know what the concentration and
> temperature is good for
> processing?
> I searched online and noticed some solution
> is mixed with water and some with Methanol.What is
> the difference between
> them?
>
> By the way,is there any special concern about store
> and disposing it after
> processing?
> Thanks a lot!
>
>
> DL
>
>
_________________________________________________________________
> Ãâ·ÑÏÂÔØ MSN Explorer:
> http://explorer.msn.com/lccn/
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.memsnet.org/


__________________________________
Do you Yahoo!?
Yahoo! SiteBuilder - Free, easy-to-use web site design software
http://sitebuilder.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
MEMStaff Inc.