Hello Kris,
There is no any metallisation on my chips. I just want to know the density
of TMAH I should use
(shallow Si etch 2-3 micron, as smooth as possible), and where I can buy it
in a cheap price.
By the way, why people add some Methanol into TMAH?
Thanks a lot!



DL
----- Original Message -----
From: "kris" 
To: "General MEMS discussion" 
Sent: Friday, September 19, 2003 8:01 AM
Subject: Re: [mems-talk] TMAH etch Si


> Hi,
>
> May i know if u have any metallisation on ur chips??
>
> Kris
> --- A: 5O  wrote:
> > Dear MEMSers,
> > I need to use TMAH etch Si for just 2-3 microns, but
> > want to be as smooth
> > as possible.
> > Dose anyone know what the concentration and
> > temperature is good for
> > processing?
> > I searched online and noticed some solution
> > is mixed with water and some with Methanol.What is
> > the difference between
> > them?
> >
> > By the way,is there any special concern about store
> > and disposing it after
> > processing?
> > Thanks a lot!
> >
> >
> > DL
> >
> >
> _________________________________________________________________
> > Cb7QOBTX MSN Explorer:
> > http://explorer.msn.com/lccn/
> >
> >
> > _______________________________________________
> > [email protected] mailing list: to unsubscribe
> > or change your list
> > options, visit
> >
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> > Hosted by the MEMS Exchange, providers of MEMS
> > processing services.
> > Visit us at http://www.memsnet.org/
>
>
> __________________________________
> Do you Yahoo!?
> Yahoo! SiteBuilder - Free, easy-to-use web site design software
> http://sitebuilder.yahoo.com
>
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Addison Engineering
Harrick Plasma, Inc.