Dear MEMS colleagues,

In one of our projects we need to CVD-deposit a homogeneous silicon-oxide layer
inside a silicon trench (aspect ratio = 200). Does anybody have experience or a
reference for a CVD deposition inside a high-aspect ratio silicon trench?

Thanks in advance.
With best regards
    Marc

______________________________________________________________________________
Zwei Mal Platz 1 mit dem jeweils besten Testergebnis! WEB.DE FreeMail
und WEB.DE Club bei Stiftung Warentest! http://f.web.de/?mc=021183


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering