Al-pyrex anodic bonding
2003-09-18
[email protected]
2003-09-22
Brubaker Chad
Al-pyrex anodic bonding
Brubaker Chad
2003-09-22
Ryan,

My first thought is that the oxide from the aluminum is getting in the way.
Even for silicon-Pyrex anodic bonding, excessive oxide can block the bonding
process. With Aluminum, it is even worse, since Al forms oxide so quickly.

My best recommendation would be to perform an oxide removal immediately prior to
bonding.  For best results, you should also perform the bonding process itself
in reducing atmosphere (such as forming gas).


Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   [email protected] [mailto:[email protected]]
Sent:   Thursday, September 18, 2003 8:51 AM
To:     [email protected]
Subject:        [mems-talk] Al-pyrex anodic bonding

Hello all,
  i am interested in developing Al-pyrex anodic bonding.  I have performed
several experiments using thin film aluminum and pyrex glass and have been only
successful a few times.  i have not been able to make my process highly
repeatable. I would appreciate advice from anyone who has had experience with
this process.

Regards.
Ryan

Ryan D. Pooran
Ph.D Candidate Microelectronics-Photonics
Mechanical Engineering Department
University of Arkansas
Fayetteville, AR 72701
Ph:479-575-4150
Fax: 479-575-6982
e-mail: [email protected]


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing