Khosla,

You need to be a bit more specific as to what your intentions are for these
materials.  Both of these materials have a wide range of application
capabilities.  AZP4620 is capable of producing coats in single layers in the
range of 5 - 33 um, with multi-layers going much thicker.  This allows
applications in surface and bulk micromachining, all the way up to wafer
bumping. SU-8 has an even greater range, with 2 um coats all the way up to 250
um (or perhaps more) possible, depending on grade of SU-8 used.

In each of these cases, the specific processing needs are going to depend on the
layer thickness and application desired.  Your best bet would be to first
contact the manufacturers of these materials:

AZP4620 - Clariant - AZ Electronic Materials (www.azresist.com)
SU-8 - MicroChem Corp. (www.microchem.com)

Best Regards,

Chad Brubaker

EV Group       invent * innovate * implement
Technology - Tel: (602) 437-9492, Fax: (602)437-9435 e-mail:
[email protected], www.EVGroup.com

This message and any attachments contain confidential or privileged information,
which is intended for the named addressee(s) only. If you have received it in
error, please notify the sender immediately and then delete this e-mail. Please
note that unauthorized review, copying, disclosing, distributing or otherwise
making use of the information is strictly prohibited.


 -----Original Message-----
From:   Ramparsad Khosla [mailto:[email protected]]
Sent:   Tuesday, September 23, 2003 5:11 AM
To:     General MEMS discussion
Subject:        [mems-talk] PHOTORESIST

Hi

Can anyone help me get the proper parameters to working with photoresist
like AZP4620 and SU-8?

Thanks a lot

KHOSLA Vicky
NUS Undergrad

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing