MEMSnet Home: MEMS-Talk: PHOTORESIST
PHOTORESIST
2003-09-23
Ramparsad Khosla
2003-09-23
Greg Reimann
2003-09-23
Brubaker Chad
PHOTORESIST
Greg Reimann
2003-09-23
Nominal parameters for SU-8 can be found in the datasheets on the right
hand side of this page:

http://www.microchem.com/products/su_eight.htm

You will probably have to tweak them, but they are a good starting
point.

I've never used AZP4620.

Greg Reimann
Boston University
Precision Engineering Research Lab

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Ramparsad Khosla
Sent: Monday, September 22, 2003 11:11 PM
To: General MEMS discussion
Subject: [mems-talk] PHOTORESIST

Hi

Can anyone help me get the proper parameters to working with photoresist
like AZP4620 and SU-8?

Thanks a lot

KHOSLA Vicky
NUS Undergrad

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Nano-Master, Inc.
The Branford Group
MEMS Technology Review