MEMSnet Home: MEMS-Talk: Does molten Indium wet SiO2 surface?
Does molten Indium wet SiO2 surface?
2003-09-25
Yuanbo Zhang
2003-09-25
Kirt & Erika Zipf-Williams
Does molten Indium wet SiO2 surface?
Kirt & Erika Zipf-Williams
2003-09-25
The Indium Corp. of America's documentation says that indium adheres to
silicon dioxide.
I cut up small pieces of sheet indium, put them on a heavily doped silicon
surface (which of course has native oxide),
and flowed a lot of current through the indium. It melted and adhered well
enough to get an ohmic contact.
Not a direct answer, but maybe it'll help.
    --Kirt Williams, Ph.D.   consultant

----- Original Message -----
From: Yuanbo Zhang 
To: 
Sent: Thursday, September 25, 2003 11:17 AM
Subject: [mems-talk] Does molten Indium wet SiO2 surface?


> Hi all,
>
> I am trying to thermally evaporate ~30nm Indium film onto SiO2
> substrate, then heat it up
>   to the melting temperature of Indium. Does anyone know if Indium wets
> SiO2 surface?
>   If it does NOT wet, how is the adhesion between Indium and SiO2? If it
> does wet, what
> kind of substrate should I use to get a non-wetting contact?
>
> Any suggestions would be greatly appreciated.
>
> Yuanbo Zhang
> Dept. of Physics, Columbia University
> 538 West 120th St., PUPIN 704
> New York, NY 10027
> Phone: (212)8540393
> Fax: (212)8540392
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Harrick Plasma, Inc.
Mentor Graphics Corporation