A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicone for bonding?
Silicone for bonding?
2003-10-01
Jalinous Esfandyari
2003-10-02
Kirt & Erika Zipf-Williams
Silicone for bonding?
Kirt & Erika Zipf-Williams
2003-10-02
> Does anyone know what the right silicone for bonding the pressure sensor
bare die on PCB is? How do I prevent the fracture and keep good adhesive?
[FLUFF TRIMMED]

Use an RTV (room-temperature vulcanizing) silicone from Dow Corning or GE,
such as RTV 730.
Young's modulus for RTVs is very low, so little (but not zero) stress gets
transmitted from the die to what it's mounted on.
I would caution you that the PCB probably has a much higher TCE than
silicon,
so thermal stress will be created as the temperature fluctuates, which will
give a false signal.
It is better to mount the die on something else like Kovar, then attach that
to the board.

    --Kirt Williams, Ph.D.  consultant


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
The Branford Group
MEMS Technology Review