Dear colleges,

I will use 20um and 50um thick device layer SOI wafer to fabricate a large
structure(2000um by 2000um square) with DRIE. To release the structure
with HF, I need to design etching holes.

I wonder what's the appropriate etching hole size and hole offset  should
I adopt to smooth the HF etching process but still keep the size(mass) of the
big structure as much as possible?

Thanks for your possible help!

Jing

MEMS Lab.,
Dept. of Mechanical Engineering,
Univ. of Maryland, College Park,
MD, 20770




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing