MEMSnet Home: MEMS-Talk: photoresist remove
photoresist remove
2003-10-02
Yilei Zhang
2003-10-03
Eric Miller
2003-10-03
Bill Moffat
2003-10-03
Michael D Martin
photoresist remove
Bill Moffat
2003-10-03
Yilei,
      Try a single wafer Oxygen + CF4 plasma reaction.  What size are your
samples and how many.  I may be able to test them free for you.  Contact me
directly.  Bill Moffat

-----Original Message-----
From: Yilei Zhang [mailto:[email protected]]
Sent: Thursday, October 02, 2003 3:01 PM
To: [email protected]
Subject: [mems-talk] photoresist remove


Dear Members:
I have some samples with photoresist (AZ5209) coating for a long time, now i
cannot
remove it by aceton, stripper, or ultrasonic cleaner. Can anyone give me some
suggestions? Thanks.

Regards,
Yilei Zhang










_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer
The Branford Group