Dear All,

I am a new-comer of MEMS area. I am suffering from KOH etching problem. My
outside convex edge has been etched to be round because I forget corner
compensation when I draw my design. I do not have any budget to order a new
mask. Is KOH+IPA will help me? What is the recipe? I am also confused what the
undercut compensation really meant in some literature.

Your help is highly apperciated.

Lydia



-------------------------------------------------
This mail sent through IMP: http://horde.org/imp/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
The Branford Group