Hi Jing,

   The size and pattern of your etch holes all depend on your requirements.

Do you have any material incompatibilities with HF which could cause
material corrossion?

More holes less etch time thus less corrosion.

Does your released structure have a curvature due to deposited materials?

You would have to consider edge effects on the structure as well as variable
etch rates which can cause small chunks of silicon to be ripped away from
either device layer due to these tensile or compressive forces.

Also for any hole pattern you choose, conduct an etch simulation (expanding
circles) which also include the edge to make sure you don't have isolated
islands of oxide left unless it is desired.

Phil Tabada

>From: Jing Liu 
>Reply-To: General MEMS discussion 
>To: [email protected]
>Subject: [mems-talk] DRIE/SOI structure releasing hole?
>Date: Thu, 2 Oct 2003 13:22:30 -0400 (EDT)
>
>Dear colleges,
>
>I will use 20um and 50um thick device layer SOI wafer to fabricate a large
>structure(2000um by 2000um square) with DRIE. To release the structure
>with HF, I need to design etching holes.
>
>I wonder what's the appropriate etching hole size and hole offset  should
>I adopt to smooth the HF etching process but still keep the size(mass) of
>the
>big structure as much as possible?
>
>Thanks for your possible help!
>
>Jing
>
>MEMS Lab.,
>Dept. of Mechanical Engineering,
>Univ. of Maryland, College Park,
>MD, 20770
>
>
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/

_________________________________________________________________
Get MSN 8 Dial-up Internet Service FREE for one month.  Limited time offer--
sign up now!   http://join.msn.com/?page=dept/dialup


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing