Hi!
   I had a question about the susceptibility of parylene to the chemicals TMAH
(tetra methyl ammonium hydroxide) & BOE (buffered oxide etch : HF+H2O +NH4F).
Parylene was deposited in hollow silicon molds & needs to be released by etching
away the silicon & some intermediate silicon dioxide. Need to know if the
chemicals would attack the exposed parylene in the process of etching silicon.
Kindly respond.
 - Asma


---------------------------------
Do you Yahoo!?
The New Yahoo! Shopping - with improved product search
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics