MEMSnet Home: MEMS-Talk: Ni electroforming (RAvindra Mukhiya)
Ni electroforming (RAvindra Mukhiya)
2003-10-02
ravindra mukhiya
2003-10-08
Sooje Cho
Ni electroforming (RAvindra Mukhiya)
Sooje Cho
2003-10-08
Hi, Ravindra

I didn't get your mail.

First you must arrange polished stainless plate or silicon(or other plates) on
which stainless thin film is coated by sputtering(or e-beam...).
Second make a SU-8 mold.
3rd  electroplate(nickelsulfamate acid solution is good)
4th  remove the SU-8(RIE, firing??)
5th  separate the electroplated mickel.


Sooje Cho
MEMSware Inc.
Tel:+82-(0)2-2281-6558
Fax:+82-(0)2-2281-6559
[email protected]
www.memsware.com
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group