MEMSnet Home: MEMS-Talk: problems with RIE grass
problems with RIE grass
2003-10-08
Jiaping Yue
2003-10-09
[email protected]
2003-10-09
Lamontagne, Boris
2003-10-09
Michael D Martin
problems with RIE grass
[email protected]
2003-10-09
Ping:

The problem might be with the aluminum hard mask you are using. The amount of
rie used during processing might be responsible for breaking down native al2o3.
This is then a very effective micromask as it doesn't etch in the presence of
fluorine. A more effective mask might be Chrome or photoresist if possible. You
can call me if you would like to discuss further. Bob Henderson 480-968-8818 x
11

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group