HI Rob,

YOu can try dipping it into dilute H2SO4 for ~15sec, then you will see the
shiny surface of copper seed layer. HOpe it helps:>

Linda:)

On Thu, 9 Oct 2003, Rob Davis wrote:

> Date: Thu, 9 Oct 2003 13:29:13 -0400
> From: Rob Davis 
> To: [email protected], [email protected], [email protected]
> Subject: [mems-talk] Copper Electroplate
>
> Greetings all, need advice.  How to minimize flash oxidation of electroplated
copper, are there any tricks or passivation agents?
>
> Thanks
> Rob Davis
> Caldus Semiconductor
> [email protected]
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
Mentor Graphics Corporation
Nano-Master, Inc.