A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: surviving temperature of crosslinked SU-8
surviving temperature of crosslinked SU-8
2003-10-16
LSWANG
2003-10-16
Christopher F. Blanford
2003-10-16
Bill Moffat
2003-10-16
ShuTing Hsu
surviving temperature of crosslinked SU-8
Bill Moffat
2003-10-16
Do not know about SU8 specifically.  With normal positive resists if you use
image reversal or silylation think very high temperatures with no distortion.
One colleague used reversal and flowed TEOS at 405 without distortion.
Silylation should give even higher temperature resistance theoretically.  I do
not have any data to confirm this.  Bill Moffat

-----Original Message-----
From: LSWANG [mailto:[email protected]]
Sent: Wednesday, October 15, 2003 5:43 PM
To: [email protected]
Subject: [mems-talk] surviving temperature of crosslinked SU-8


Hi,
Does anyone have some idea about what is the highest
temperature crosslinked SU-8 structure can stand with
losing the feature resolution. 300C or higher?
thanks
Lisen

__________________________________
Do you Yahoo!?
The New Yahoo! Shopping - with improved product search
http://shopping.yahoo.com

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.