In a capacitively coupled RIE with 6" electrodes, we run oxygen plasmas
for etching polymers at 200-300 mTorr and 300 W. To clean the chamber,
use oxygen at 400mTorr and 300-400W.

-Mike


>>> [email protected] 10/17/03 9:33 AM >>>
I have done a RIE process on a silicon wafer in a CHF3(80 sccm,3.8*10^-2
mbar) plasma for 1 hour for my degree thesis.
I'm looking for a metod to remove the polymer film due to the process on
the surface. I have read that it is possible with an oxigen plasma RIE
process but I don't know what parameters to use.I'm also interested in a
metod to clean the RIE chamber, if it is necessary in this case.
Please, help me. Thanks.


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
University Wafer
MEMStaff Inc.