Leonard,

I do a 100 watt, 100mT, 5 minute, O2 run after every SF6 run I do.  Once a month
I'll do this run, wipe the chamber down with methanol, and then do another O2
run.  I seems to keep my chamber clean.

Brent

[email protected] wrote:

> I have done a RIE process on a silicon wafer in a CHF3(80 sccm,3.8*10^-2 mbar)
plasma for 1 hour for my degree thesis.
> I'm looking for a metod to remove the polymer film due to the process on the
surface. I have read that it is possible with an oxigen plasma RIE process but I
don't know what parameters to use.I'm also interested in a metod to clean the
RIE chamber, if it is necessary in this case.
> Please, help me. Thanks.
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
garber.vcf (text/x-vcard, 361 bytes)
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Harrick Plasma, Inc.
The Branford Group
MEMStaff Inc.