Q: Ti wet etching
Linda LW Chow
2003-10-18
Hi,

You can try buffered HF. :>

Linda:)

On Fri, 17 Oct 2003, t. hamano wrote:

> Date: Fri, 17 Oct 2003 11:10:35 -0500
> From: t. hamano 
> Reply-To: General MEMS discussion 
> To: [email protected]
> Subject: [mems-talk] Q: Ti wet etching
>
> Hi all!
> I would like to ask you about the recipe of Ti etchant.  We are going to
> etch a <50 nm thick Ti layer on epitaxial barium titanate.  Since this
> material must be unfamiliar with you, you don't forget about it.  I just
> want to know what kinds of etchant you usually fix for Ti etching.
>
> Thanks a lot in advance.
>
> T. Sophie Hamano
>
>
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Mentor Graphics Corporation
University Wafer