A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Low stress silicon nitride.
Low stress silicon nitride.
2003-10-21
Elena Sidorov -BlueBird
2003-10-21
Chris Kovach
2003-10-21
Michael Huff
2003-10-21
Bill Flounders
2003-10-21
Almog Ronen
2003-10-21
Eric Miller
2003-10-21
M. Mubeen Almoustafa
Low stress silicon nitride.
Chris Kovach
2003-10-21
Sidorov Elena,

We offer low stress nitride.  Can you give me more specifications on the
film?

Chris

____________________________________________
Chris Kovach, Ph.D.
Executive Director
The Center for Micro and Nano Processing
The Microfabrication Laboratory
The Electronics Design Center

Case Western Reserve University
10900 Euclid Avenue
Bingham Building, Rm 107A
Cleveland, OH,  44106-7200

Ph: (216) 368-3628
Fax: (216) 368-8738
[email protected]




-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Elena Sidorov -BlueBird
Sent: Tuesday, October 21, 2003 4:10 AM
To: [email protected]
Subject: [mems-talk] Low stress silicon nitride.



Hello,

 I'm looking for a vendors that can deposit >5000A um low stress nitride
for membranes fabrication. Thanks in advance for your information.

Sidorov Elena, BlueBird Optical MEMS


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
MEMStaff Inc.