Elena Sidorov -BlueBird
2003-10-21
Chris Kovach
2003-10-21
Michael Huff
2003-10-21
Bill Flounders
2003-10-21
Almog Ronen
2003-10-21
Eric Miller
2003-10-21
M. Mubeen Almoustafa
Low stress silicon nitride.
Michael Huff
2003-10-21


Sidorov,

I would encourage you to go to the MEMS Exchange
web site.  We have over 40 foundries in our
network, many of which can deposit low-stress
LSN on a variety of size substrates and stress
levels.

You can find the info at:

https://www.mems-exchange.org/

Let me know if you have any questions.


-Michael

****************************************************
Dr. Michael A. Huff
Director of the MEMS Exchange
Corporation for National Research Initiatives
1895 Preston White Drive
Reston, Virginia  20191

Tel:            703-262-5318

Visit us at:    http://www.mems-exchange.org










>Hello,
>
>  I'm looking for a vendors that can deposit >5000A um low stress nitride for
>membranes fabrication. Thanks in advance for your information.
>
>Sidorov Elena, BlueBird Optical MEMS
>
>
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.memsnet.org/
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing