MEMSnet Home: MEMS-Talk: Low stress silicon nitride.
Low stress silicon nitride.
2003-10-21
Elena Sidorov -BlueBird
2003-10-21
Chris Kovach
2003-10-21
Michael Huff
2003-10-21
Bill Flounders
2003-10-21
Almog Ronen
2003-10-21
Eric Miller
2003-10-21
M. Mubeen Almoustafa
Low stress silicon nitride.
Bill Flounders
2003-10-21
The UC Berkeley Microlab provides this film through MEMS Exchange.
See: http://www.mems-exchange.org/catalog/
or contact me directly if you need additional information.
Thank you.
Bill Flounders
Microlab Technology Manager


  can provide this film.
Please contact me

Elena Sidorov -BlueBird wrote:
> Hello,
>
>  I’m looking for a vendors that can deposit >5000A um low stress nitride for
> membranes fabrication. Thanks in advance for your information.
>
> Sidorov Elena, BlueBird Optical MEMS
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing