ERIC SIMONE
2003-10-23
taya sunil
PMMA as microcantilever material
2003-10-23
Samir Kagadkar
2003-10-21
Tomblin, Graham (OH32)
low temperature anodic bonding
Tomblin, Graham (OH32)
2003-10-21
Eric
I haven't seen a low temperature anodic bond, generally the mismatch problem is
"minimized " be selecting a glass
closely matched with silicon, there are a number around, any good glass plate
supplier should be able to help.
Alternatively you may be able to use a low temperature glass frit.
Graham

-----Original Message-----
From: ERIC SIMONE [mailto:[email protected]]
Sent: Monday, October 20, 2003 9:20 PM
To: [email protected]
Subject: [mems-talk] low temperature anodic bonding


I was wondering if anyone has a good recipe for low temperature anodic bonding,
where by low I mean no higher than 200
or 250C. I'm trying to bond a microscope cover glass to a Si wafer but do not
want to heat up too high, since the
thermal coefficient is different for this glass, compared to the Si (thus when
they cool there will be cracking) Thanks
much.


_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.