MEMSnet Home: MEMS-Talk: Low stress silicon nitride.
Low stress silicon nitride.
2003-10-21
Elena Sidorov -BlueBird
2003-10-21
Chris Kovach
2003-10-21
Michael Huff
2003-10-21
Bill Flounders
2003-10-21
Almog Ronen
2003-10-21
Eric Miller
2003-10-21
M. Mubeen Almoustafa
Low stress silicon nitride.
Eric Miller
2003-10-21
Sidorov,

We can deposit both LPCVD (up to 4" wafers) and PECVD (up to 8" wafers) low
stress nitride.  Please let me know the specifics of your process i.e.
thickness uniformity, thickness target, number of wafers, and I will be
happy to send you a quotation.

Eric Miller
Manger of Program Operations
WTC Microfab Lab
206 616-3855
[email protected]  http://microfab.watechcenter.org

----- Original Message -----
From: "Elena Sidorov -BlueBird" 
To: 
Sent: Tuesday, October 21, 2003 2:10 AM
Subject: [mems-talk] Low stress silicon nitride.


>
> Hello,
>
>  I’m looking for a vendors that can deposit >5000A um low stress nitride
for
> membranes fabrication. Thanks in advance for your information.
>
> Sidorov Elena, BlueBird Optical MEMS
>
>
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.memsnet.org/
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Harrick Plasma, Inc.
The Branford Group
Tanner EDA by Mentor Graphics