     Regan Nayve,

     As part of my thesis work I discovered that the addition of a metal or
     rare earth element to the KOH solution increases the etch ratio of
     silicon to silicon dioxide:

     "An Integrated Pressure Sensor for In-vivo Use", Ph.D. thesis,
     Stanford University, Stanford, CA, June 1987.

     Regards,

     Brent E. Burns
     Integrated Micro Sensors Group, manager
     Northrop Grumman ESID
     Hawthorne, CA
     213-600-5526
     [email protected]



______________________________ Reply Separator _________________________________
Subject: Si KOH etching
Author:  Navye Regan  at INTERNET
Date:    11/11/97 11:42 AM


ISI MEMS Electronic Discussion Group members,

I am working on wafer-through etching of Si substrate
using KOH. I am wondering if there is a method of
achieving smooth(mirror-like)111 surface. And does anyone
know about regulating SiO2 mask etching rate in KOH?
I would appreciate it very much if you could refer
books or published materials regarding the above subject.
Thanks in advance.


Best regards,

Regan Nayve
Fuji Xerox, NMD Dept.
e-mail (business): [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics