Dear all,

I would appreciate if someone can help me about gas mixture composition about
dry etching of sputtered tin oxide films on SiO2, with RIE or ICP, possibly with
medium-high selectivity vs silicon dioxide.

Thanks in advance to All

Dr. Giovanni Morelli