Re: Anisotropic c-Si RIE (Jobert van Eisden)
2003-10-28
[email protected]
Re: Anisotropic c-Si RIE (Jobert van Eisden)
[email protected]
2003-10-28
Jobert,

You can try:
- to use a typical Bosch Process and reduce the gas pulsed times and gas
flows, at low source power and pressure. With this type of process, we are
able to achieve a RMS roughness lower than 20nm for a 30um deep etch,
- to use an unpulsed process with a mixture of SF6 and C4F8.

Jean - Marc Thevenoud
Process Engineer, Alcatel ICP etcher
Phone: 781 331 4200
email: [email protected]





reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
The Branford Group