MEMSnet Home: MEMS-Talk: metal? etch mask for TMAH
metal? etch mask for TMAH
2003-10-29
Karin Buchholz
2003-10-30
Shile
2003-11-18
Martyna
2003-11-18
Massimiliano Decarli
2003-11-19
David Nemeth
SiO2 sputtering rate
2003-11-21
Oray Orkun Cellek
In search for another room-temp casting material on silicon
2003-11-18
Wei-han J. Wu
metal? etch mask for TMAH
Shile
2003-10-30
One nice thing about etching Silicon with TMAH is the very low SiO2 etch
rate.  If the "Oxide" you mention is silicon dioxide, why don't you just
use that as a mask?  A couple of thousand Angstroms should be adequate.

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Karin Buchholz
Sent: Wednesday, October 29, 2003 7:45 AM
To: [email protected]
Subject: [mems-talk] metal? etch mask for TMAH

Dear all,


Does anybody have a suggestion for a TMAH etch mask which I can remove
without etching Oxide?

I need to etch trough the bulk of a Si Wafer (600µm) covered with Oxide
on top which will also serve as an etch stop.
I do not want to destroy it when removing the mask.

Will a gold layer be stable to the long etching time needed? If yes,
what is the best sticking layer and how thick does the gold need to be?


Thank you for your help,

Karin

--
mailto: [email protected]



_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group