Trisha Browne
Localized stress measurement
2003-10-31
Linda LW Chow
Sputtering/spraying for Photogrammetry
Trisha Browne
2003-10-31
You can use stroboscopic interferometry to measure the deformation, and
then you don't have to coat your samples-

If you have any questions, please give me a call.


Regards-

Trisha


Patricia Browne
Product Manager - MEMS Test & Characterization Tools
Veeco Metrology
2650 E Elvira Rd
Tucson, AZ 85706
P: 520-741-1044X1091
[email protected]


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
ramji dhakal
Sent: Wednesday, October 29, 2003 1:32 PM
To: General MEMS discussion
Subject: [mems-talk] Sputtering/spraying for Photogrammetry

Hi MEMS workers,

I want to measure the deformation of some MEMS scale
or a bit larger structures by Photogrammetry. I need
to have a good distribution of grey areas and white
areas in the images. For this, I have to spray some
tiny dot particles. I need a sprayer of that capacity.
Also, an appropriate spray material would be required.
I tried to use some powders like Titanium oxide and
some other commercially available things but they do
not seem to work for that level. Could anyone suggest
me a way out?

Is it possible to sputter something? It should not
make a continuous deposit, what I need is a contrast
between the different points..

Thanks in advance for your help..
Ramji

=====
Ramji Dhakal

M S Mechanical Engineering,
SUNY Binghamton, NY

__________________________________
Do you Yahoo!?
Exclusive Video Premiere - Britney Spears
http://launch.yahoo.com/promos/britneyspears/

_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.memsnet.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.
The Branford Group