will HF damage Chrome layer?
2003-11-02
Yilei Zhang
2003-11-03
Isaac Wing Tak Chan
2003-11-03
David Nemeth
2003-11-03
Kirt & Erika Zipf-Williams
2003-11-05
Paolo Tassini
will HF damage Chrome layer?
Kirt & Erika Zipf-Williams
2003-11-03
> Can anyone tell me whether chrome layer can survive in HF etching sio2? if
> not, is there any other SiO2 etchant will not damage Chrome? thanks.
>
> Regards,
> Yilei Zhang

Our measured etch rate in 5:1 BHF is < 0.3 nm/min for sputtered Cr and 0
nm/min for evaporated Cr,
so yes, Cr will survive.
    --Kirt Williams, Ph.D.   consultant


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
MEMS Technology Review