borosilicate glass etch rates in HF
2003-11-04
Sarah McQuaide
2003-11-05
Kirt & Erika Zipf-Williams
borosilicate glass etch rates in HF
Kirt & Erika Zipf-Williams
2003-11-05
> What are typical etch rates for borosilicate glass in HF?
> Please reply to:
> [email protected]
> Thank you!

There are many formulations of borosilicate glass.
One common one in MEMS is Pyrex 7740,
which is 81% SiO2, 13% B2O3, 4% Na2O, and 2% Al2O3.
For Pyrex 7740, our measured etch rate in 5:1 BHF is 43 nm/min.
Curiously, this is much slower than the ER for fused quartz (pure SiO2), at
130 nm/min.
    --Kirt Williams, Ph.D.   consultant


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.